MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ametek SEALVAR® F-15 Alloy or UNS K94610 Nickel-Iron-Cobalt Strip
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Nickel Alloy

Material Notes: AMETEK’s Nickel-Iron-Cobalt strip, SEALVAR®, is a high quality alloy used primarily for making hermetic seals with harder glasses and ceramics. SEALVAR® is distinguished from competitive F-15 alloy by its higher purity, more closely controlled chemistry, and very low carbon level.

Advantages

  • Reproducible Low Level Of Reactive Impurity Elements: Improved die wear; Improved soldering; Improved bonding (cladding); Predictable oxidation: Rate; Adherence; Uniformity; Predictable response to other chemical surface treatment steps; Lower work hardening rate; Improved metal flow in coining operations; Reduced stress on glass or ceramic
  • Low Carbon: 0.01% Max.; 0.004% Nom.: Improved die wear; Predictable response to bright dip; Elimination and/or simplification of decarburization heat treatment; Reduced sealing bubbles; Retention of fine grain size and resulting improved fatigue life and gold plated surface cosmetics
  • Higher Electrical Conductivity (~10%): Improved current flow.
  • Higher Thermal Conductivity (~10%): Improved heat dissipation
  • Lower Softening Point (~150%): Lower annealing temperatures; Reduced interdiffusion in clad metal processing

Information provided by AMETEK Inc.

Vendors:
Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield, 0.2% offset
  • Elongation at Break
  • Modulus of Elasticity
  • Electrical Resistivity
  • Curie Temperature
  • Heat of Fusion
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Copper, Cu
  • Iron, Fe, Balance
  • Magnesium, Mg
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Silicon, Si
  • Titanium, Ti
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.