MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Morgan Advanced Ceramics Hicast Super Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Hicast Super is a 2800°F (1538°C) product containing a graded kaolin calcine aggregate. It is designed for internal or external high frequency vibration only. The densely packed structure produces low permeability and excellent abrasion resistance. Hicast Super has excellent resistance to alkali attack. Method of installation is vibratory cast.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramic
Vendors:
Available Properties
  • Density, ASTM C-134, fired
  • Deformation, ASTM C16, under hot load, dried 24hrs @ 104°C
  • Modulus of Rupture, ASTM C 583, hot
  • Modulus of Rupture, ASTM C 583, hot
  • Modulus of Rupture, ASTM C 583, hot
  • Modulus of Rupture, ASTM C 583, hot
  • Modulus of Rupture, ASTM C 133, dried
  • Modulus of Rupture, ASTM C 133, dried
  • Compressive Strength, ASTM C133, Cold Crushing Strength, dried 24 hrs at 104°C
  • Compressive Strength, ASTM C133, Cold Crushing Strength, dried 5hrs at 816°C
  • Compressive Strength, ASTM C133, Cold Crushing Strength, fired 5hrs @ temperature use limit
  • Abrasion, ASTM C704, cm3, loss, fire at 815°C
  • Thermal Conductivity, ASTM C201
  • Thermal Conductivity, ASTM C201
  • Thermal Conductivity, ASTM C201
  • Thermal Conductivity, ASTM C201
  • Maximum Service Temperature, Air
  • Shrinkage, ASTM C 113, dried
  • Shrinkage, ASTM C 113, fired
  • Shrinkage, ASTM C 113, fired
  • Moisture Content, recommended, casting by vibrating
  • Shelf Life
  • Al2O3
  • CaO
  • Fe2O3
  • NaO2, as Na2O
  • SiO2
  • TiO2
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.