| Polymerization System: Cold emulsion Polymerization Emulsifier: Mixed Acid Soap Stabilizer: Staining Coagulant: Acid Extender: Highly aromatic oil, 37.5 phr Characteristics: Superior processing properties with extender oil, good wear, tear and cracking resistance Application: Tire, footwear, conveyor belts, camelback, molded and extruded industrial goods Test Recipe, ASTM D-3185 Parts Taipol SBR-1712E - 137.50 Zinc oxide - 3.00 Stearic acid - 1.00 Sulfur - 1.75 HAF black(IRB#9) – 68.75 TBBS - 1.38 Total – 213.38 Information provided by TSRC Corporation |