MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Ensinger TECASINT™ 2022 Polyimide, Black, 15% Graphite (PI)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications. TECASINT™ 2011 is very pure, and exhibits low outgassing. It is also characterized by it’s long term thermal stability, outstanding wear resistance, high creep resistance, and strength up to its continuous use temperature of 536° F. TECASINT™ 2021 contains 15% graphite and is also available for applications requiring improved wear resistance & lower coefficient of friction.
  • Superior high temperature characteristics (TECASINT™ 2000 series can operate up to 536° F continuously)
  • Excellent long-term thermal stability
  • Outstanding bearing and wear properties (at elevated temperatures, TECASINT™ 2000 formulations offer superior wear rates)
  • Excellent creep resistance
  • High strength and stiffness properties
  • High purity characteristics (only extremely low levels of extractables and ionic impurities are apparent in TECASINT™ 2011)
  • Good chemical resistance (TECASINT™ 2000 series is not attacked by common solvents or fuels and is acceptable for use in contact with many acids)

TECASINT™ 2000 series with their superior physical properties, are ideal for applications in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries. TECASINT™ shapes are excellent candidates for high purity applications in the semiconductor processing industry. Typical components produced from TECASINT™ applications include seals, thrust washers, bushings and wear pads in transportation/off-highway equipment, insulating and support elements in electrical welding and brazing equipment, and wafer-handling components in the harsh environment of semiconductor plasma ovens. Pump and valve seals, vanes, and piston rings are also commonly produced from TECASINT™ series materials.

Information Provided by Ensinger Inc.

Key Words: PI CS 15
Vendors:
Available Properties
  • Density, DIN 53 479
  • Water Absorption, DIN EN ISO 62, 24 hours in water
  • Water Absorption, DIN EN ISO 62, 24 hours in water
  • Hardness, Shore D, DIN 53 505
  • Tensile Strength, EN ISO 527
  • Elongation at Break, EN ISO 527
  • Tensile Modulus, EN ISO 527
  • Flexural Strength, EN ISO 178
  • Flexural Modulus, EN ISO 178
  • Flexural Strain at Yield, EN ISO 178
  • Compressive Yield Strength, EN ISO 604
  • Compressive Strength, EN ISO 604
  • Compressive Modulus, EN ISO 604
  • Charpy Impact Unnotched, EN ISO 179
  • Charpy Impact, Notched, EN ISO 179
  • Compression Set, EN ISO 604, Compression at Break
  • CTE, linear, DIN 53 752
  • CTE, linear, DIN 53 752
  • Specific Heat Capacity
  • Thermal Conductivity, ISO 8302
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi), DIN 53 461
  • Glass Transition Temp, Tg, DMTA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.