MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.

Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum service temperature of 80°C/176°F; Can cure at temperatures from 120°C to 175°C/248°F to 347°F; Suitable for application by spatula or extrusion; Very low volatile content.
Applications: Bonding segments of honeycomb core; Bonding edges of honeycomb core to structural edge members in bonded sandwich panels; Panel section bonding.

Vendors:
Available Properties
  • Density, Foamed/Cured Density; Cure Cycle: 20 min @ 175°C/347°F
  • Density, Foamed/Cured Density; Cure Cycle: 30 min @ 150°C/302°F
  • Density, Foamed/Cured Density; Cure Cycle: 60 min @ 120°C/248°F
  • Density, EN542
  • Compressive Yield Strength, ASTM D695, Block Compression; Cure Cycle: 20 min @ 175°C/347°F
  • Compressive Yield Strength, ASTM D695, Block Compression; Cure Cycle: 30 min @ 150°C/302°F
  • Compressive Yield Strength, ASTM D695, Block Compression; Cure Cycle: 60 min @ 120°C/248°F
  • Shear Strength, DMS2180, Short Beam Shear; Dry; 60 min @ 120°C
  • Shear Strength, DMS2180, Short Beam Shear; Dry; 30 min @ 150°C
  • Shear Strength, DMS2180, Short Beam Shear; Dry; 20 min @ 175°C
  • Shear Strength, Hexcel IS202, Double Lap Shear - 1000 hours @ 80°C/176°F, 100% RH; 30 min @ 150°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 20 min @ 175°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 30 min @ 150°C
  • Shear Strength, Hexcel IS202, Double Lap Shear - 1000 hours @ 80°C/176°F, 100% RH; 20 min @ 175°C
  • Shear Strength, Hexcel IS202, Double Lap Shear - 1000 hours @ 80°C/176°F, 100% RH; 60 min @ 120°C
  • Shear Strength, Hexcel IS202, Double Lap Shear; Dry; 60 min @ 120°C
  • Shear Strength, Hexcel IS202, Double Lap Shear; Dry; 20 min @ 175°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 60 min @ 120°C
  • Shear Strength, Hexcel IS202, Double Lap Shear; Dry; 30 min @ 150°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 20 min @ 175°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 60 min @ 120°C
  • Shear Strength, Hexcel IS202, Double Lap Shear; Dry; 60 min @ 120°C
  • Shear Strength, Hexcel IS202, Double Lap Shear; Dry; 20 min @ 175°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 20 min @ 175°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 30 min @ 150°C
  • Shear Strength, Hexcel IS202, Double Lap Shear; Dry; 30 min @ 150°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 30 min @ 150°C
  • Shear Strength, EN2667-2, Tube Shear; Dry; 60 min @ 120°C
  • Glass Transition Temp, Tg, EN 6064, E' onset; Cure Cycle: 60 min @ 120°C/248°F
  • Glass Transition Temp, Tg, EN 6064, E' onset; Cure Cycle: 30 min @ 150°C/302°F
  • Glass Transition Temp, Tg, EN 6064, E' onset; Cure Cycle: 20 min @ 175°C/347°F
  • Cure Time
  • Cure Time
  • Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.