MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Categories: Polymer; Thermoplastic

Material Notes: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and application after application. It will not weaken or crack after years of exposure to heat and ozone. This provides long service in a wide range of applications such as gasketing, abrasion-resistant sleeving and cable insulation. Performance formulated for on-the-job reliability, Norprene® handles temperatures from -75°F (-60°C) to 275°F (135°C), allowing the use of one material with a broad range of temperatures. It is heat sealable and can be joined without fittings. It also has excellent resistance to inorganic (acids and bases) fluids. With its outstanding flexural fatigue resistance and high temperature capability, Norprene® Industrial Grade Tubing outlasts and outperforms virtually all other general service tubings in peristaltic and vacuum pump applications.

Features/Benefits:
  • Superior weathering
  • Abrasion resistant
  • Outstanding flexural fatigue resistance
  • Wide temperature range (-75°F to 275°F)
  • Low gas permeability versus rubber tubing
  • Ozone and UV light resistant
Typical applications include Soap and Disinfectant Dispensing, Printing Ink Transfer, Caustic Dispensing, Plating and Etching Chemicals, Wastewater Sampling, Glass and Window Wash Systems, Vacuum Pumps, Cable Insulation, Abrasion Resistant Sleeving.
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792-98
  • Water Absorption, ASTM D570-98, 24 hours at 23°C
  • Hardness, Shore A, ASTM D2240-97, 15 seconds
  • Tensile Strength, Yield, ASTM D412-98
  • Elongation at Break, ASTM D412-98
  • 100% Modulus, ASTM D412-98
  • 300% Modulus, ASTM D412-98
  • Tear Strength, ASTM D1004-94, Initial Tear Strength
  • Compression Set, ASTM D395-98 Method B, Constant Deflection, for 22 hrs.
  • Tensile Set, ASTM D412-98
  • Dielectric Strength, ASTM D149-97
  • Maximum Service Temperature, Air
  • Brittleness Temperature, ASTM D746-98
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.