| Hostacom ERC 161N is a 15% talc filled PP copolymer, with very good flowability, good dimensional stability, excellent impact/stiffness balance and good scratch resistance. This product is also available in other colors, new colors can be developed depending on customer requirements. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts; Instrument Panels; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Abrasion Resistance; Good Color Stability; Good Flow; Good Impact Resistance; Good Surface Finish; High Stiffness; Low Density; Low to No Odor; Scratch Resistant; UV Resistant Information provided by LyondellBasell. |