MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Aluminum 2048-T851 Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A92048; Aluminium 2048; AA2048; Al2048-T851
Vendors:
Available Properties
  • Density, AA; Typical
  • Hardness, Brinell, 500 kg load with 10 mm ball. Calculated value.
  • Hardness, Knoop, Converted from Brinell Hardness Value
  • Hardness, Rockwell A, Converted from Brinell Hardness Value
  • Hardness, Rockwell B, Converted from Brinell Hardness Value
  • Hardness, Vickers, Converted from Brinell Hardness Value
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate, Plate; Transverse
  • Tensile Strength, Ultimate, Plate; Longitudinal
  • Tensile Strength, Ultimate, Plate; Transverse
  • Tensile Strength, Ultimate, Plate; Longitudinal
  • Tensile Strength, Ultimate, Plate; Longitudinal
  • Tensile Strength, Ultimate, Plate; Transverse
  • Tensile Strength, Ultimate, Plate; Longitudinal
  • Tensile Strength, Ultimate, Plate; Short transverse
  • Tensile Strength, Ultimate, Plate; Transverse
  • Tensile Strength, Yield
  • Tensile Strength, Yield, Plate; Longitudinal
  • Tensile Strength, Yield, Plate; Transverse
  • Tensile Strength, Yield, Plate; Longitudinal
  • Tensile Strength, Yield, Plate; Transverse
  • Tensile Strength, Yield, Plate; Transverse
  • Tensile Strength, Yield, Plate; Longitudinal
  • Tensile Strength, Yield, Plate; Short transverse
  • Tensile Strength, Yield, Plate; Longitudinal
  • Tensile Strength, Yield, Plate; Transverse
  • Elongation at Break, In 5 cm
  • Elongation at Break, Plate; Short transverse
  • Elongation at Break, Plate; Transverse
  • Elongation at Break, Plate; Longitudinal
  • Elongation at Break, Plate; Transverse
  • Elongation at Break, Plate; Longitudinal
  • Elongation at Break, Plate; Longitudinal
  • Elongation at Break, Plate; Transverse
  • Elongation at Break, Plate; Longitudinal
  • Reduction of Area, Plate; Short transverse
  • Reduction of Area, Plate; Transverse
  • Reduction of Area, Plate; Transverse
  • Reduction of Area, Plate; Longitudinal
  • Reduction of Area, Plate; Longitudinal
  • Reduction of Area, Plate; Transverse
  • Reduction of Area, Plate; Longitudinal
  • Reduction of Area, Plate; Transverse
  • Reduction of Area, Plate; Longitudinal
  • Creep Strength, Plate; Longitudinal
  • Creep Strength, Plate; Longitudinal
  • Creep Strength, Plate; Longitudinal
  • Creep Strength, Plate; Longitudinal
  • Creep Strength, Plate; Longitudinal
  • Creep Strength, Plate; Longitudinal
  • Rupture Strength, Plate; Longitudinal
  • Rupture Strength, Plate; Longitudinal
  • Rupture Strength, Plate; Longitudinal
  • Rupture Strength, Plate; Longitudinal
  • Rupture Strength, Plate; Longitudinal
  • Rupture Strength, Plate; Longitudinal
  • Tensile Modulus, Compressive modulus in is typically about 2% higher for Al alloys
  • Tensile Modulus, Plate; Transverse
  • Tensile Modulus, Plate; Longitudinal
  • Tensile Modulus, Plate; Longitudinal
  • Tensile Modulus, Plate; Transverse
  • Tensile Modulus, Plate; Longitudinal
  • Tensile Modulus, Plate; Transverse
  • Tensile Modulus, Plate; Longitudinal
  • Tensile Modulus, Plate; Transverse
  • Tensile Modulus, Plate; Short transverse
  • Compressive Yield Strength, Plate; Transverse
  • Compressive Yield Strength, Plate; Longitudinal
  • Compressive Yield Strength, Plate; Longitudinal
  • Compressive Yield Strength, Plate; Transverse
  • Compressive Yield Strength, Plate; Transverse
  • Compressive Yield Strength, Plate; Longitudinal
  • Compressive Yield Strength, Plate; Longitudinal
  • Compressive Yield Strength, Plate; Transverse
  • Compressive Strength
  • Compressive Strength
  • Compressive Strength
  • Compressive Strength
  • Compressive Strength
  • Compressive Strength
  • Compressive Strength
  • Compressive Strength
  • Compressive Modulus
  • Compressive Modulus
  • Compressive Modulus
  • Compressive Modulus
  • Compressive Modulus
  • Compressive Modulus
  • Compressive Modulus
  • Compressive Modulus, Plate; Longitudinal
  • Compressive Modulus, Plate; Longitudinal
  • Compressive Modulus, Plate; Transverse
  • Compressive Modulus, Plate; Transverse
  • Compressive Modulus, Plate; Longitudinal
  • Compressive Modulus, Plate; Transverse
  • Compressive Modulus, Plate; Transverse
  • Compressive Modulus, Plate; Longitudinal
  • Poissons Ratio, Estimated from trends in similar Al alloys.
  • Fatigue Strength
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Notched, Kt=3.0; R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fatigue Strength, Plate; Axial fatigue (longitudinal); Unnotched, R=0.1
  • Fracture Toughness, K(IC) in T-L Direction
  • Fracture Toughness, K(IC) in L-T Direction
  • Shear Modulus, Estimated from similar Al alloys.
  • Shear Strength
  • Charpy Impact, Transverse
  • Charpy Impact, Longitudinal
  • Electrical Resistivity, T851 Temper
  • CTE, linear
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity, T851 Temper
  • Melting Point, Estimated from trends in similar Al alloys.
  • Solidus, Estimated from trends in similar Al alloys.
  • Liquidus
  • Aluminum, Al, As remainder
  • Copper, Cu
  • Iron, Fe
  • Magnesium, Mg
  • Manganese, Mn
  • Other, each
  • Other, total
  • Silicon, Si
  • Titanium, Ti
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.