MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Sandvik Bioline F562/F562LTi Wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik Bioline F562 is a nonmagnetic Nickel-cobalt base alloy that has a unique combination of properties: ultra high strength, toughness, ductility and excellent corrosion resistance. Sandvik Bioline F562LTi is the low titanium version of Sandvik Bioline F562. The alloy is cold worked to obtain strength level of 17902205 MPa (260 to 320 ksi). It can also be aged in the work hardened condition to achieve higher strengths. A leading material for permanent implants, Sandvik Bioline F562 is vacuum melted in multiple steps for extreme cleanliness. Sandvik Bioline F562 is resistant to corrosion in hydrogen sulfide, salt water and other chloride solutions as well as mineral acids (nitric, hydrochloric, sulfuric). In addition, it has exceptional resistance to crevice and stress corrosion cracking having been operationally proven in sea water and hostile environments. For medical use, Sandvik delivers F562 with the highest surface finish (Medical class) in order to maximize the fatigue strength, which is critical in implant devices such as lead wires for pacemakers and heart valve supports.

Information provided by Sandvik

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B, Annealed
  • Hardness, Rockwell C, Cold worked
  • Hardness, Rockwell C, Aged 593°C- 4 hrs
  • Tensile Strength, Ultimate, Annealed
  • Tensile Strength, Ultimate, Hot worked
  • Tensile Strength, Ultimate, Aged 593°C- 4 hrs
  • Tensile Strength, Yield, Annealed
  • Tensile Strength, Yield, Hot worked
  • Tensile Strength, Yield, Aged 593°C- 4 hrs
  • Elongation at Break, Hot worked
  • Elongation at Break, Aged 593°C- 4 hrs
  • Elongation at Break, Annealed
  • Modulus of Elasticity, Annealed
  • Modulus of Elasticity, Cold worked and aged
  • Poissons Ratio, Annealed; Calculated
  • Poissons Ratio, Cold worked and aged; Calculated
  • Shear Modulus, Cold worked and aged
  • Shear Modulus, Annealed
  • CTE, linear
  • Thermal Conductivity
  • Chromium, Cr
  • Cobalt, Co
  • Molybdenum, Mo
  • Nickel, Ni
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.