SYNTHOS PS HI 562E is high-impact polystyrene (HIPS) with properties suitable for thermoforming. It is a thermoplastic material designed for extrusion and thermoforming. SYNTHOS PS HI 562E is an opaque plastic. Product has a form of lens granules of diameter 2,5 to 4 mms. Product may contain small amounts of granulate finer than that mentioned above of irregular shapes. Presence of any mechanical impurities in the granulate is not allowed.