MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dow Versify™ 3010 PE
Categories: Polymer; Thermoplastic

Material Notes: Product Description: Versity™ 3010 is a propylene ethylene copolymer with a medium melt flow rate manufactured with Dow’s Advanced Molecular Catalyst technology. It is suitable for cast film blown film and BOPP. It is an excellent sealant and is particularly suitable for use in BOPE structures. It has excellent compatibility with PP and is a useful agent to bring toughness and temperature performance.
Main Characteristics:
  • Free flow pellet
  • Medium Melt Flow Rate
  • Excellent compatibility with PP
  • Soft polypropylene<
Applications:
  • Blown film
  • Cast film
  • BOPE
  • BOPP
  • Sealant
Compiles with: US FDA 21 CFR 176.170©; US FDA FCN 909

Availability: Asia Pacific; Europe; Latin America; North America

Agency Ratings: FDA 21 CFR 176.170©; FDA FCN 909

Form: Pellets

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ISO 1183
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240, Injection Molded
  • Tensile Strength at Break, ASTM D638, Compression Molded
  • Elongation at Break, ASTM D638, Compression Molded
  • Flexural Modulus, ASTM D790, 1% Secant, Compression Molded
  • Melting Point
  • Vicat Softening Point, ASTM D1525
  • Gloss, ASTM D523, 60°, Compression Molded
  • Gloss, ASTM D523, 20°, Compression Molded
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.