| Praseodymium Fluoride, is the main raw materials for making Praseodymium Metal, and also applied in color glasses and enamels; when mixed with certain other materials, Praseodymium produces an intense clean yellow color in glass. Praseodymium is present in the rare earth mixture whose Fluoride forms the core of carbon arc lights which are used in the motion picture industry for studio lighting and projector lights. Doping Praseodymium in Fluoride glass allows it to be used as a single mode fiber optical amplifier. Applications: is the main raw materials for making Praseodymium Metal, and also applied in color glasses and enamels; when mixed with certain other materials, praseodymium produces an intense clean yellow color in glass Solubility: Insoluble in water, moderately soluble in strong mineral acids Molecular Formula: PrF3 Room temperature, dry, sealedAlfa Chemistry Materials product group: Metal Manufacturer data sheet |