MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Daikin OPTODYNE UV-1100 Optical Adhesive
Categories: Polymer; Adhesive

Material Notes: OPTODYNE is a reliable UV curable optical adhesive with controlled refractive index.

Introduction: Transparent ultraviolet (UV) curing type optical adhesive based on fluorinated epoxy and fluorinated acrylate resin; It is used to connect optical fibers requiring optically optimal refractive index matching as well as adhesion fixing function; Highly reliable adhesive with excellent adhesion and workability

Information provided by Daikin.

Vendors:
Available Properties
  • Specific Gravity, Before-curing
  • Specific Gravity, Post-curing
  • Moisture Absorption, Saturated, 85% -curing
  • Water Absorption at Saturation, Post-curing
  • Water Absorption at Saturation, Post-curing
  • Viscosity, Before-curing
  • Hardness, Shore D, Post-curing
  • Tensile Modulus, Post-curing, Dynamic viscoelasticity
  • Adhesive Bond Strength, Pyrex glass, after 100 cycles, 90% RH/6 hr/1 cycle, Post-curing
  • Adhesive Bond Strength, Pyrex glass, Initial, 85% RH, Post-curing
  • Adhesive Bond Strength, Pyrex glass, Initial, 90% RH/6 hr/1 cycle, Post-curing
  • Adhesive Bond Strength, Pyrex glass, 6 weeks, 85% RH, Post-curing
  • Adhesive Bond Strength, Pyrex glass, after 500 cycles, 90% RH/6 hr/1 cycle, Post-curing
  • Adhesive Bond Strength, Pyrex glass, 4 weeks, 85% RH, Post-curing
  • Adhesive Bond Strength, Pyrex glass, after 300 cycles, 90% RH/6 hr/1 cycle, Post-curing
  • Glass Transition Temp, Tg, Dynamic viscoelasticity, Post-curing
  • Flash Point, Before-curing
  • Refractive Index, Before-curing
  • Refractive Index, Post-curing
  • Refractive Index, Post-curing
  • Transmission, Visible, Post-curing
  • Transmission, Visible, Post-curing
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Daikin Industries

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.