MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Tra-Con Tra-Bond JL01 High Viscosity High Temperature Fiber Optic Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND JL01 is a high viscosity, two-component epoxy formulation that is suggested for bonding fiber optic bundles, potting glass fibers, and terminating single or multi-channel fiber optic connectors. The unique color change of this material ensures proper mixing and curing. TRA-BOND JL01 develops strong, tough, mechanically stable bonds to a wide variety of fiber optic and optical materials that includes most metals, ceramics, glass and many plastics. It has good impact and thermal shock resistance, and yields excellent low stress, pot-and-polish connections that do not piston during cycle tests. It is also resistance to water and weathering, vapors and gases, most petroleum products, and an extended range of organic and inorganic environments.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Viscosity, Mixed (rv #7, 10 rpm)
  • Hardness, Shore D, 30 min @ 150°C
  • Adhesive Bond Strength, Lap shear, alum to alum, 15 min @ 100°C
  • Adhesive Bond Strength, Lap shear, alum to alum, 30 min @ 150°C
  • Glass Transition Temp, Tg, Ultimate Tg
  • Cure Time
  • Cure Time
  • Pot Life
  • Working Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.