| Hostacom TRC 2016N is a 10% talc filled PP copolymer, with high flowability, good impact/stiffness balance, high UV resistance and very good scratch resistance. Low emissions and low odor makes it the preferable choice for all kind of interior trim parts. Advanced technologies allow for a significant reduction of mineral filler which contributes to reduction of final part weight. Product is available as a customized color matched, pellet form. This grade is delivered in C12A50 color version. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: High Flow; Low Density Information provided by LyondellBasell. |