MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Master Bond EP48TC Two Part Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • High thermal conductivity filler
  • Applicable in very thin bond lines
  • Attains exceptionally high bond strength
  • Unsurpassed heat transfer capabilities
Product Description: Master Bond EP48TC is a breakthrough material pertaining to thermal management applications of epoxies. This system utilizes a unique combination of special high thermal conductive fillers and is capable of being applied in bond lines as thin as 10-15 microns. Typically, thermal conductive epoxies cannot be applied in these kinds of thin sections. Since the thermal conductivity is high, and the bond lines thin, the ultimate thermal resistance is very low. The lower the thermal resistance, the better it is for heat transfer properties. Thermal resistance is calculated from the formula: R=t/K (where “R” is the thermal resistance; “t”, the thickness and “K” the thermal conductivity of the material). Using real numbers, when standard alumina filled thermally conductive epoxy is applied in 50 micron thick sections, the thermal resistance is 30-35 x 10-6 K•m2/W. With EP48TC, the thermal resistance is significantly lower: 5-7 x 10-6 K•m2/W, because of the filler and its ability to be effectively applied in sections of 10-15 microns in width. Simply put, this epoxy is second to none when transferring heat. EP48TC is a user friendly system with a forgiving 100 to 40 mix ratio by weight, or 100 to 50 by volume. Upon mixing, It has a long open time with a paste consistency. The epoxy cures at room temperature in 4-7 days or in 4-6 hours at 150-200°F. To optimize properties, the recommended cure is overnight at room temperature followed by 3-5 hours at 150-200°F. The system bonds well to a wide variety of substrates, including metals, composites, glass, ceramics and many plastics. Other positives include a very low coefficient of thermal expansion, low shrinkage upon curing and exceptional dimensional stability. EP48TC has first rate electrical insulation properties over the wide service temperature range from -100°F to +300°F. The color of Parts A and B is gray. Notably, EP48TC passes NASA low outgassing testing. This very special system can be used in applications in the aerospace, electronic, optical, specialty OEM and many other high technology industries, where optimum thermal transfer properties are a necessity.

Product Advantages:

  • High thermal conductivity and electrical insulation values
  • Exceptionally low coefficient of thermal expansion
  • Unsurpassed low thermal resistance
  • NASA low outgassing approved

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Specific Gravity, Part B
  • Specific Gravity, Part A
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Elongation at Break
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.