MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Resinlab® EP1200LV Casting Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the requirements of UL Standard 94 for a horizontal burn rating at 1/4" thickness. It was especially formulated to a 1:1 mix ratio for use in MMD equipment or side-by side cartridges. It contains abrasive aluminum oxide filler which can introduce wear considerations for wetted components. It shows very good stability in side-by-side cartridges. Cure is normally achieved at room temperature although an elevated cure schedule can be used to reach final properties quickly. This product was designed to be cured in less than 2 hours at 65oC for ease of processing and also to reduce viscosity. It was especially formulated to a 1A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. Times and temperatures from 2 hours at 65oC to 10 minutes at 100oC are typical for small castings (less than 100 grams).

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors:
Available Properties
  • Specific Gravity, TM R050-16, Part A
  • Specific Gravity, TM R050-16, Mixed
  • Specific Gravity, TM R050-16, Part B
  • Water Absorption, TM R050-35
  • Viscosity, TM R050-12, Part A, RVT, #6, 20 rpm.
  • Viscosity, TM R050-12, Part B, RVT, #6, 20 rpm.
  • Viscosity, Mixed
  • Hardness, Shore D
  • Tensile Strength at Break, TM R050-36
  • Tensile Strength, Ultimate, TM R050-36
  • Tensile Strength, Yield, TM R050-36
  • Elongation at Break, TM R050-36
  • Tensile Modulus, TM R050-36
  • Compressive Yield Strength, TM R050-38
  • Compressive Strength, TM R050-38, Break
  • Compressive Strength, TM R050-38, Ultimate
  • Compressive Modulus, TM R050-38
  • Adhesive Bond Strength, Lap Shear-Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor
  • CTE, linear, Below Tg
  • CTE, linear, Above Tg
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time
  • Cure Time
  • Pot Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.