Description: ICORENE 150-1500 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is enhanced with ICOPOwer, RotoGO, ColorBrite and Veriform. The base resin is FDA approved and is fully stabilized to UV8 level. Key Characteristics: high stiffness, high toughness, good processing. Applications: This ICORENE® grade is particularly suitable for use in kayak applications.Information provided by ICO Polymers. This LyondellBasell product line was formerly a product of ICO Polymers and of A. Schulman. |