MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Syensqo (Solvay Specialty Polymers) Omnix® 4050 High Performance (HPPA), 50% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: 50% glass fiber, high performance polyamide

Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used in automotive, consumer goods, E/E, and construction. Components injection molded from Omnix® 4050 display exceptional mechanical properties and excellent surface appearance even after moisture adsorption.

- Black: Omnix® 4050 BK 000
- Natural: Omnix® 4050 NT 000

Applications: Automotive Electronics; Electrical/Electronic Applications; Machinery Maintenance/Repair

Features: Fast Molding Cycle; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Paintable

- Typical values shown tested on Dry as Molded samples.
- Standard Packaging and Labeling: Omnix® 4050 resin is packaged in foil lined, multiwall paper bags containing 25 kg (55 pounds) of material. Individual packages will be plainly marked with the prod

Injection notes: Drying:
- Omnix® 4050 resin is shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It should be dried before molding because excessive moisture content will result in reduced mechanical properties and processing issues, such as excessive nozzle drooling, foaming and splay visible on the molded parts.
- Recommended drying conditions are as follows:
-- Type of drier: Desiccant
-- Temperature: 80°C (175°F)
-- Time: 4-12 hours
-- Dew point: -30°C (-22°F) or lower
-- Polyamides oxidize in the presence of oxygen at high temperatures. Therefore drying temperatures above 80°C should be avoided, particularly for light colors or color-controlled parts.
Injection Molding:
- Omnix® 4050 resin can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure. The melt temperature should be between 275°C and 290°C (527°F and 554°F). Generally this can be achieved with barrel temperatures from 250°C (482°F) in the rear zone gradually increasing to 285°C (545°F) in the front zone. Mold temperature should be between 80° and 120°C (176° and 248°F).
- Set injection pressure to give rapid injection. Adjust holding pressure to one-half injection pressure. Set hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled.
Storage:
- Omnix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container.

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ISO 62
  • Moisture Absorption, ISO 62, 50% RH
  • Water Absorption at Saturation, ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Linear Mold Shrinkage, Transverse, ISO 294-4
  • Tensile Strength, Yield, ISO 527-2
  • Elongation at Break, ISO 527-2
  • Tensile Modulus, ISO 527-2
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Melting Point, ISO 11357-3
  • Flammability, UL94
  • Rear Barrel Temperature
  • Front Barrel Temperature
  • Melt Temperature, Injection
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.