MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Covestro Bayflex® LSR 10 Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Bayflex LSR 10 is a solid elastomer which has a flexural modulus of 17,500 psi* at room temperature.

Properties / Applications: Bayflex LSR 10 is a solid elastomer which has a flexural modulus of 17,500 psi* at room temperature. It is processed on reaction injection molding (RIM) equipment and is used for glass encapsulation of windows. This system combines rapid demold times, excellent integrity at demold, and outstanding physical properties. The Bayflex LSR 10 system was developed to add a weather-resistant grade to our range of window encapsulation systems. In some cases, the weatherability of this system eliminates the need for post-painting or in-mold coatings. This product is available only in black. Bayflex LSR 10 is a formulated RIM system supplied as two reactive liquid components. Component A is a diphenylmethane diisocyanate (MDI) prepolymer, and component B is a polyether polyol. As with any product, use of the Bayflex LSR 10 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors:
Available Properties
  • Specific Gravity, Polyol (Component B)
  • Specific Gravity, Isocyanate (Component A)
  • Viscosity, Isocyanate (Component A)
  • Viscosity, Polyol (Component B)
  • Hardness, Shore A
  • Hardness, Shore A
  • Hardness, Shore D
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • Flexural Modulus
  • Flexural Modulus
  • Flexural Modulus
  • Tear Strength
  • Compression Set, 25% deflection
  • Flash Point, Isocyanate (Component A)
  • Flash Point, Polyol (Component B)
  • Mold Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.