MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil Bicor® 100 LTSC OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTSC) delivers a low seal initiation temperature, wide operating range for applications where accurate heat control is a problem or dwell times vary because of frequent machine speed changes. LTSC’s acrylic surface is excellent for surface printing and provides good aroma barrier.

Availability: Latin America, North America and South America

Key Features:

  • Wide sealing range with a low minim seal temperature (MST)
  • Excellent seal strength and hot tack
  • Robust performances on horizontal flowpack machines
  • Excellent humidity seal retention on LTSC side
  • Good flavor and aroma barrier
  • Outstanding optical properties
  • Ideal support for normal ink systems
Features:
  • Acrylic Coated
  • Flavor & Aroma Barrier
  • Humidity Resistant
  • In Lamination Lap Sealable
  • LTS Coated
  • Very Broad Seal Range
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Confectionery, Chocolate
  • Confectionery, Gum
  • Confectionery, Sugar
  • Frozen Food
  • Health and Beauty Care
  • Household and Detergents
  • Tobacco
Uses:
  • HFF Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil Chemical

Vendors:
Available Properties
  • Water Vapor Transmission, ExxonMobil Method, 90% RH
  • Thickness, ExxonMobil Method, Nominal
  • Coating Weight, ExxonMobil Method
  • Coefficient of Friction, ExxonMobil Method
  • Film Tensile Strength at Break, MD, ExxonMobil Method, 20 in/min, 2.0 in Jaw Separation
  • Film Tensile Strength at Break, TD, ExxonMobil Method, 20 in/min, 2.0 in Jaw Separation
  • Shrinkage, MD, ExxonMobil Method
  • Shrinkage, TD, ExxonMobil Method
  • Haze, ExxonMobil Method
  • Gloss, ExxonMobil Method, 45º, Acrylic Surface
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.