MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Fibre Glast Duratec 1040 Clear Hi-Gloss Gel Coat Additive
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: #1040 can be mixed 1:1 with regular gel coat to reduce viscosity, porosity, and permit a complete open air cure. The reduction in viscosity allows gel coat to be sprayed controllably through siphon and HVLP equipment, reducing sanding and polishing time. Below the waterline repairs still need the addition of #71 Styrene Wax for maximum hardness.

Features:
  • Low Porosity - when used for repairs, blending the additive with gelcoat produces a low porosity surface
  • Reduced orange peel - the low viscosity of the blend results in a smooth finish that is easily sanded
  • Improved properties - for mold surfaces, the blending of the additive with tooling gelcoat creates a higher heat distortion temperature, improved gloss retention, increased impact resistance and reduced subsurface porosity.
  • Superior Finish - when blended one-to-one with gelcoats, the additive created an air-cure enamel-like coating. No air-dry additive is required. When used for gelcoat repair, surfaces are restored to like-new condition.

    Information provided by Fibre Glast Developments Corporation.

Vendors:
Available Properties
  • Brookfield Viscosity, Brookfield RVF #2 Spindle at 20 rpm
  • Transmission, Visible, clear; thickness not quantified
  • Gel Time, Value for a 100g mass, catalyzed at 2 percent with MEKP - 2%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Fibre Glast Developments Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.