| Hostacom TRC 352N E1 D52999 is a 20% talc filled PP copolymer, with excellent blooming resistance at elevated temperatures, very good impact/stiffness balance, very good processability, very good scratch resistance and very good surface appearance. This grade is delivered in Color D52999. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts; Instrument Panels; Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Good Moldability; High Impact Resistance; Non Blooming; Scratch Resistant; UV Resistant Information provided by LyondellBasell. |