MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
LyondellBasell Adflex Q 100 F Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adflex Q 100 F is a thermoplastic polyolefin, which is mainly used by our customers for the extrusion of blown film. It is also suitable for sheet extrusion. Adflex Q 100 F features very high softness and very low modulus. It does not contain any slip or anti-blocking agents Adflex Q 100 F is used for the production of soft hygienic film and heavy duty film, as well as for the modification of LDPE or LLDPE to increase mechanical characteristics, puncture resistance, and to allow further down gauging. It can be easily processed on conventional LDPE or LLDPE blown film lines.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe; North America; South & Central America

Application: Agriculture Film; Bags & Pouches; Barrier Film; Breathable Film; Collapsible Tubes; Film Wrap; Food Packaging Film; Heavy Duty Packaging; Hygiene Film; Interior Automotive Applications; Lamination Film; Shrink Film; Stretch Hood; Surface Protection Film; TPO Foils and Skins

Market: Flexible Packaging; Rigid Packaging

Processing Method: Blown Film; Calendaring; Double Bubble; Extrusion Blow Molding; Extrusion Flat-die; Sheet; Thermoforming

Attribute: Good Flexibility; Good Processability; Good Puncture Resistance; Good Tear Strength; Low Temperature Impact Resistance; Low Transparency; Soft

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Density, ISO 1183-1, Method A
  • Melt Flow, ISO 1133-1
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, ISO 527-1, -2
  • Elongation at Break, ISO 527-1, -2
  • Flexural Modulus, ISO 178
  • Charpy Impact, Notched, ISO 179, Complete Break
  • Charpy Impact, Notched, ISO 179, Partial Break
  • Charpy Impact, Notched, ISO 179
  • Melting Point, ISO 11357-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75B-1, -2, Unannealed
  • Vicat Softening Point, ISO 306, A/50
  • Gloss, ASTM D2457, 60°
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.