MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Evonik VESTAMID® NRG 2101 YE Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® NRG 2101 YE is a high molecular grade PA 12 material developed by Evonik. Its superior performance characteristics make it a good choice for expanding the use of thermoplastic piping systems at higher operating pressures and larger diameters to replace metallic piping systems in a safe and cost effective manner. Besides extending the operating pressure limits of thermoplastic piping systems, VESTAMID® NRG 2101 YE offers many of the same benefits, and in most instances more superior performance, as conventional PE piping systems.
  • Tough and durable
  • Corrosion resistant
  • Resistant to heavy hydrocarbons
  • High resistance to Slow Crack Growth and Rapid Crack Propagation
  • Increased installation efficiencies
  • Worry free performance
These characteristics make the VESTAMID® NRG 2101 yellow material a good choice when selecting appropriate thermoplastic piping materials in extending gas distribution infrastructure. The manufacturer recommends a processing temperature between 230°C (446°F) and 260°C (500°F) - in some cases up to 280°C (536°F) - during the injection molding and extrusion process. The mold temperature should be within a range of 60°C (140°F) to 100°C (212°F). Drying at 80°C (176°F) for 2 hours to 4 hours before processing is recommended. Polyamide 12 is a high performance thermo-plastic polymer with increased performance characteristics that translates into safe operations over the life of the installed pipe- line. It has a considerable record of safe and proven experience in many demanding applications, including fuel lines in passenger cars, air brake tubing in trucks and off-shore applications. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Sustainable, Industry and Engineering, Energy, Oil and Gas
Sustainability: Sustainable electricity
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering, Fatigue resistance, Oil / fuels
Electrical: Insulating
Additives: Unfilled
Applications: Tube and hose
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: Halogen-free, Phosphorus-free, High impact strength, Semi-crystalline, Environmental stress crack resistance, Light-stabilized, U.V. stabilized, High heat resistant, High viscosity
Features: Weldable, High melt strength
Color: Yellow
Additives: Heat stabilizer
Delivery form: Spherical pellets
Chemical Resistance: Solvent resistance, Grease resistance, Oil resistance, Ozone resistance, Aging resistance, Fuel resistance, General chemical resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, Sim to ISO 62
  • Moisture Absorption, Sim to ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Melt Flow, ISO 1133
  • Hardness, Shore D, ISO 7619-1
  • Tensile Strength at Break, ISO 527
  • Tensile Strength, ISO 527
  • Tensile Stress, ISO 527
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Break, ISO 527, mat. nom. strain at br., etB
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Flexural Strength, ISO 178, at conv. Deflection
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Flexural Strain at Break, ISO 178, at flexural strength
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: P/C
  • Volume Resistivity, IEC 62631-3-1
  • Surface Resistance, IEC 62631-3-2, circular electrodes
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Constant, IEC 62631-2-1
  • Dielectric Strength, IEC 60243-1, Conditioned, AC, S20/S20, t.
  • Dielectric Strength, IEC 60243-1, Dry, AC, S20/S20, t.
  • Dissipation Factor, IEC 62631-2-1
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • Melting Point, ISO 11357-1/-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1/-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306, 50 K/h
  • Vicat Softening Point, ISO 306, 50 K/h
  • Glass Transition Temp, Tg, ISO 11357-1/-2
  • Melt Temperature, ISO 294, Injection Molding
  • Melt Temperature
  • Mold Temperature, ISO 294, Injection Molding
  • Mold Temperature
  • Injection Velocity, ISO 294, Injection Molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.