| Emulprene 1012CR is a crumb version of a high viscosity hot emulsion styrene-butadiene copolymer, polymerized using fatty acid emulsifier and coagulated with salt-acid. It is very light color product stabilized with a non-staining antioxidant. Between 4% and 12% of Calcium Carbonate is used as dusting agent Uses: Emulprene 1012CR is the high molecular weight version of Emulprene 1006CR, it dissolves readily in solvents and particularly useful as binder for fibrous materials and adhesives where increased cohesive strength is desired. Information provided by Dynasol Group. |