MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
Overview of materials for Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors:
Available Properties
  • Density, Average value: 1.41 g/cc Grade Count:507
  • Density, Average value: 0.620 g/cc Grade Count:1
  • Filler Content, Average value: 32.5 % Grade Count:8
  • Volatile Organic Compounds (VOC) Content, Average value: 96.8 g/l Grade Count:12
  • Water Absorption, Average value: 0.531 % Grade Count:92
  • Particle Size, Average value: 32.0 µm Grade Count:5
  • Viscosity, Average value: 119000 cP Grade Count:765
  • Viscosity, Average value: 60000 cP Grade Count:39
  • Linear Mold Shrinkage, Average value: 0.00419 cm/cm Grade Count:28
  • Outgassing - Total Mass Loss, Average value: 0.747 % Grade Count:19
  • Outgassing - Total Mass Loss, Average value: 0.600 % Grade Count:1
  • Outgassing - Total Mass Loss, Average value: 0.600 % Grade Count:1
  • Hardness, Shore A, Average value: 62.8 Grade Count:14
  • Hardness, Shore D, Average value: 76.6 Grade Count:667
  • Hardness, Shore D, Average value: 59.5 Grade Count:13
  • Tensile Strength, Ultimate, Average value: 42.9 MPa Grade Count:564
  • Tensile Strength, Ultimate, Average value: 9.47 MPa Grade Count:18
  • Tensile Strength, Yield, Average value: 14.8 MPa Grade Count:50
  • Tensile Strength, Yield, Average value: 6.30 MPa Grade Count:7
  • Elongation at Break, Average value: 16.9 % Grade Count:286
  • Elongation at Break, Average value: 1.21 % Grade Count:1
  • Elongation at Yield, Average value: 5.56 % Grade Count:6
  • Modulus of Elasticity, Average value: 3.29 GPa Grade Count:344
  • Modulus of Elasticity, Average value: 3.45 GPa Grade Count:8
  • Flexural Yield Strength, Average value: 128 MPa Grade Count:57
  • Flexural Yield Strength, Average value: 45.8 MPa Grade Count:4
  • Flexural Modulus, Average value: 10.9 GPa Grade Count:17
  • Flexural Modulus, Average value: 6.11 GPa Grade Count:1
  • Compressive Yield Strength, Average value: 106 MPa Grade Count:212
  • Compressive Yield Strength, Average value: 28.7 MPa Grade Count:5
  • Compressive Modulus, Average value: 8.46 GPa Grade Count:52
  • Poissons Ratio, Average value: 0.321 Grade Count:5
  • Shear Modulus, Average value: 1.96 GPa Grade Count:5
  • Shear Modulus, Average value: 2.10 GPa Grade Count:3
  • Shear Strength, Average value: 18.9 MPa Grade Count:280
  • Shear Strength, Average value: 17.0 MPa Grade Count:120
  • Shear Strength, Average value: 17.0 MPa Grade Count:15
  • Shear Strength, Average value: 17.0 MPa Grade Count:15
  • Adhesive Bond Strength, Average value: 19.0 MPa Grade Count:566
  • Adhesive Bond Strength, Average value: 17.5 MPa Grade Count:107
  • Adhesive Bond Strength, Average value: 17.5 MPa Grade Count:3
  • Adhesive Bond Strength, Average value: 17.5 MPa Grade Count:3
  • Izod Impact, Notched, Average value: 0.797 J/cm Grade Count:25
  • Gardner Impact, Average value: 21.7 J Grade Count:5
  • Coefficient of Friction, Average value: 1.69 Grade Count:4
  • Peel Strength, Average value: 7.76 kN/m Grade Count:248
  • Peel Strength, Average value: 4.83 kN/m Grade Count:26
  • Peel Strength, Average value: 4.83 kN/m Grade Count:3
  • Peel Strength, Average value: 4.83 kN/m Grade Count:3
  • Electrical Resistivity, Average value: 1.27e+15 ohm-cm Grade Count:486
  • Electrical Resistivity, Average value: 9.96e+12 ohm-cm Grade Count:21
  • Surface Resistance, Average value: 2.36e+16 ohm Grade Count:7
  • Dielectric Constant, Average value: 5.49 Grade Count:369
  • Dielectric Constant, Average value: 5.32 Grade Count:6
  • Dielectric Constant, Average value: 5.32 Grade Count:10
  • Dielectric Constant, Average value: 5.32 Grade Count:10
  • Dielectric Strength, Average value: 18.1 kV/mm Grade Count:305
  • Dissipation Factor, Average value: 0.0336 Grade Count:138
  • Dissipation Factor, Average value: 0.0784 Grade Count:6
  • Dissipation Factor, Average value: 0.0784 Grade Count:11
  • Dissipation Factor, Average value: 0.0784 Grade Count:11
  • Arc Resistance, Average value: 85.8 sec Grade Count:6
  • CTE, linear, Average value: 56.7 µm/m-°C Grade Count:419
  • CTE, linear, Average value: 159 µm/m-°C Grade Count:38
  • Specific Heat Capacity, Average value: 0.300 J/g-°C Grade Count:3
  • Thermal Conductivity, Average value: 1.87 W/m-K Grade Count:231
  • Thermal Conductivity, Average value: 0.185 W/m-K Grade Count:9
  • Thermal Conductivity, Average value: 0.185 W/m-K Grade Count:5
  • Thermal Conductivity, Average value: 0.185 W/m-K Grade Count:5
  • Maximum Service Temperature, Air, Average value: 164 °C Grade Count:751
  • Deflection Temperature at 0.46 MPa (66 psi), Average value: 58.0 °C Grade Count:7
  • Deflection Temperature at 1.8 MPa (264 psi), Average value: 49.0 °C Grade Count:3
  • Heat Distortion Temperature, Average value: 113 °C Grade Count:6
  • Minimum Service Temperature, Air, Average value: -73.4 °C Grade Count:621
  • Glass Transition Temp, Tg, Average value: 97.6 °C Grade Count:300
  • Decomposition Temperature, Average value: 406 °C Grade Count:4
  • Flammability, UL94, Grade Count:5
  • Flash Point, Average value: 99.8 °C Grade Count:42
  • Refractive Index, Average value: 1.55 Grade Count:65
  • Transmission, Visible, Average value: 86.9 % Grade Count:33
  • Processing Temperature, Average value: 70.2 °C Grade Count:78
  • Cure Time, Average value: 2420 min Grade Count:488
  • Cure Time, Average value: 136 min Grade Count:625
  • Cure Time, Average value: 136 min Grade Count:3
  • Cure Time, Average value: 136 min Grade Count:3
  • Tack-Free Time, Average value: 150 min Grade Count:12
  • Pot Life, Average value: 2480 min Grade Count:614
  • Pot Life, Average value: 57.5 min Grade Count:3
  • Silver, Ag, Average value: 70.7 % Grade Count:3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.