MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Thermal Ceramics Kao-Tex Woven Specialty Tape 1000
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kao-Tex 1000 textile products are made from a highly textured form of silica and are coated on one side with a proprietary treatment. They are especially designed and developed for temperatures up to 1000°F (538°C).

Kao-Tex 1000 textile products have properties which include excellent tensile strength, outstanding abrasion resistance and low thermal conductivity.

The cloth has excellent seam strength for sewing and handling which is required for the fabrication of items such as gloves and mittens.

The rope is available in two different constructions – twisted and braided.

Kao-Tex 1000 textile products have improved performance over asbestos textiles in five main areas: softer hand and feel, better thermal insulating properties than asbestos material of the same weight, better dimensional stability, abrasion resistance, and strength. These advantages result from the interaction of three factors: the use of highly textured yarn, the density of the weave, and the coated surface treatment.

Applications:

  • Welding curtains
  • Fire curtains
  • Oven curtains
  • Drop curtains
  • Stress relieving blankets
  • Welding blankets
  • Safety blankets
  • Thermal insulation blankets
  • Expansion joints
  • Piping insulation
  • Electrical insulation
  • Gas and liquid filtration
  • Laminates
  • Gaskets and seals
  • Safety garments
  • Gloves and mittens
  • Aprons
  • Spats
  • Sleeves
  • Cable and wire insulation (thermal and/or electrical)
  • Hose insulation
  • Fuel line insulation
  • Door and oven gasketing.
  • Woodburning stove seals
  • Features:

  • Designed for asbestos replacement applications at temperatures up to 1000°F (538°C)
  • Wide variety of widths and thicknesses to meet the needs of most applications
  • Bolt hole tapes make good gaskets
  • Tadpole tapes make good seals which resist abrasion and maintain strength and shape
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors:
    Available Properties
    • Specific Gravity
    • Moisture Absorption
    • Dielectric Constant
    • Dielectric Strength
    • Melting Point
    • Maximum Service Temperature, Air
    • Al2O3
    • Alkalis
    • B2O3
    • CaO
    • MgO
    • SiO2
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.