| Base Polymer: Polyamide 66 Filler/Additive System: Special filler Special Features: Thermal conductive, electrically insulating, heat ageing stabilization Market Segment: Automotive, Machinery, Electrical and Electronic, Lighting Application Area: Radiator systems, cooling system Typical Applications: Housings, functional components, plugs/connectors, lamp sockets Information provided by Albis Plastics |