| Hifax TYC 007P E G52A28 is a 22% talc filled PP copolymer, with superior melt flow rate, high rigidity, and excellent processability. Product is available as a customized color matched, pellet form. This grade is delivered in G52A28 color version. This product is also available in other colors, new colors can be developed depending on customer requirements. Availability: Europe Application: Bumpers Market: Automotive Processing Method: Injection Molding Attribute: High Flow Information provided by LyondellBasell. |