| LNP LUBRICOMP OCL36AXP compound is based on Polyphenylene Sulfide (PPS) - branched resin containing 30% carbon fiber and 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Wear resistant,Electrically Conductive,Structural Information provided by SABIC |