MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Borealis BorSafeā„¢ ME3440-W MDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: BorSafe ME3440-W is a bimodal polyethylene compound produced by the advanced Borstar technology. The product is a medium-density polyethylene compound in pellet form and contains a combination of stabilizers and carbon black to ensure a reliable long-term stability and UV-resistance. BorSafe ME3440-W is classified as an MRS 8.0 material (PE80).

Applications:

  • Cable protection pipes
  • Irrigation pipes
  • Drinking water
  • Relining
  • Gas distribution
  • Sheets and profiles
  • Industrial applications
BorSafe ME3440-W is recommended for pressure pipe systems in the application fields above.

Specifications: BorSafe ME3440-W is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures. EN 12201; ISO 4427; EN 1555; ISO 4437; EN ISO 15494

BorSafe ME3440-W provides an improved performance level in terms of drinking water related requirements such as migration limits. The sensoric properties like taste & odor are regularly monitored for the compound to ensure a high constant level of quality. The material shows excellent mechanical toughness and crack resistance also at lower temperatures. Thanks to the molecular structure, it offers outstanding extrudability and good melt strength, supporting a problem-free extrusion process to tight tolerances.

Information provided by Borealis AG

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Oxidative Induction Time (OIT), ISO 11357-6
  • Carbon Black Loading, ISO 6964
  • Carbon Black Loading, ISO 18553, dispersion
  • Melt Flow, ISO 1133-1
  • Storage Temperature
  • Tensile Strength, Yield, ISO 527-2, 50 mm/min
  • Elongation at Break, ISO 527-2, 50 mm/min
  • Tensile Modulus, ISO 527-2, 1 mm/min
  • Processing Temperature, Cylinder
  • Die Temperature
  • Melt Temperature
  • Head Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.