MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Excellent clarity and UV stable with good melt strength. Pre-drying: 2 hours at 104°C (220°F) in dehumidifying hopper dryer

Uses: Extrusion: Cable jacket, hose/tube, profile and film and sheet

Information provided by Lubrizol.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Hardness, Shore A, ASTM D2240
  • Hardness, Shore D, ASTM D2240
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412/D638
  • 300% Modulus, ASTM D412/D638
  • Modulus of Rigidity, ASTM D1053
  • Modulus of Rigidity, ASTM D1053
  • Modulus of Rigidity, ASTM D1053
  • Modulus of Rigidity, ASTM D1053
  • Modulus of Rigidity, ASTM D1053
  • Flexural Modulus, ASTM D790
  • Tear Strength, ASTM D470, Split
  • Tear Strength, ASTM D624, Die C
  • Taber Abrasion, mg/1000 Cycles, ASTM D3389 B, CS-17, 1000 g
  • Compression Set, ASTM D395
  • Compression Set, ASTM D395
  • Tensile Set, ASTM D412/D638, 200% elongation
  • Vicat Softening Point, ASTM D1525
  • Transformation Temperature, by DSC
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Adapter Temperature
  • Die Temperature, Zone 2
  • Die Temperature, Zone 1
  • Screw Speed
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Lubrizol (former Noveon)

Category Notes
Plastic
Thermoplastic Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.