MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.
Superior Flux Superior No. 153 Zinc-Based Bromide Radiator Assembly Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Zinc-Based, Bromide-Based Flux for Copper-Brass Radiator Assembly
  • Excellent Torch Soldering and Header Dipping Flux
  • Unique Hybrid Combination Limits Green Corrosion after Soldering
  • Highly Concentrated Formulation to Permit Great Dilution
  • Very Heat Stable Formulation to Tolerate Wide Range of Torch Heating Conditions
Description: Superior No. 153 is a zinc-based, bromide-based, inorganic salt type flux, specifically designed for high temperature copper-brass radiator assembly soldering. The high concentration of the Superior No. 153 flux allows for a great amount of dilution resulting in huge savings for the production operation. Superior No. 153 leaves residue that is easily removed with hot water or specialty cleaning chemistry (available from Superior). Its unique hybrid chemistry limits brass turning green after soldering.

Applications: Superior No. 153 was formulated specifically for a wide range of torch soldering copper-brass radiator assembly operations. The Superior No. 153 formulation works well with all soft solders used for radiator assembly from very high lead-based solders to lead-free solders. Normal flux application is total immersion of the brass part or flux brush application to the part.

Information provided by Superior Flux

Vendors:
Available Properties
  • Specific Gravity
  • Density
  • Surface Tension
  • Processing Temperature, Soldering Range
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

solder replacement adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.