| Hostacom HYC 665T BLACK is a 10% talc filled PP homopolymer, with high flowability and high stiffness. Product is available as non color matched, black, pellet form. Availability: Asia-Pacific Application: Automotive Parts; Underhood Market: Automotive Processing Method: Injection Molding Attribute: High Flow; High Stiffness Information provided by LyondellBasell. |