MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Thermal Ceramics BTU-Panel 1208/16
Categories: Ceramic

Material Notes: BTU-BLOCK products are a family of microporous insulation designed for use in high temperature industrial applications. Microporous insulation is a very high thermal efficiency material which has a thermal conductivity less than that of still air. These materials, consisting of fine diameter heat resistant particles, reinforcement fibers and high temperature radiation blockers, address the primary modes of heat transfer in a novel way compared to traditional refractories. These components are appropriately sized and configured to create a microporous structure. This structure limits the number and movements of air particles, and creates a material of exceptionally low thermal conductivity. At elevated temperatures, the radiation blockers are employed to minimize radiation heat transfer by again proper sizing and distribution.

Features:

  • Extremely low thermal conductivity and heat loss
  • High compressive strength
  • Fiberglass encapsulation provides flexural strength and surface for bonding (1200°F [649°C] use limit)
  • Special facing allows use limit up to 1800°F (982°C)
  • Applications:

  • OEM
  • High temperature industrial
  • Fire protection
  • Vending machines
  • Appliances
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors:
    Available Properties
    • Density, Core
    • Compressive Yield Strength, ASTM C165, Resistance to compression at 10% deformation; 16 pcf
    • Compressive Yield Strength, ASTM C165, Resistance to compression at 20% deformation; 16 pcf
    • Compressive Yield Strength, ASTM C165, Resistance to compression at 30% deformation; 16 pcf
    • Compressive Yield Strength, ASTM C165, Resistance to compression at 40% deformation; 16 pcf
    • Compressive Yield Strength, Resistance to compression at 50% deformation; 16 pcf
    • Thermal Conductivity, ASTM C210
    • Thermal Conductivity, ASTM C210
    • Thermal Conductivity, ASTM C210
    • Maximum Service Temperature, Air, Glass cloth
    • Maximum Service Temperature, Air, Specialty fabric
    • Maximum Service Temperature, Air
    • Shrinkage, ASTM C356
    • Shrinkage, ASTM C356
    • Shrinkage, ASTM C356
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    none

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.