| Emulprene 1500 is a cold styrene – butadiene copolymer, using rosin acid as emulsifier, coagulated by salt-acid system and stabilized with a non-staining antioxidant Uses: Emulprene 1500 is used as raw material in tire, shoe sole and in various industrial products. Information provided by Dynasol Group. |