MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Covestro Platilon® 2102 A Polyurethane (Ester) Film
Categories: Polymer; Film

Material Notes: Product Description: PlatilonU is the trade name for extruded thermoplastic polyurethane (TPU) films made by Epurex Films. The range currently includes aromatic TPU based on polyester and polyether.

Properties: PlatilonU films are noted for the following properties:

  • high abrasion resistance
  • flexibility over a wide temperature range
  • high resistance to oils, greases and solvents
  • good weathering resistance
  • good microbial and hydrolysis resistance of polyether TPU
  • good resistance to high-energy radiation
  • free of plasticisers
  • breathable: watertight, but high water vapour transmission rate
  • good adhesion to foams, adhesives, inks and many substratesApplications: The wide range of properties of PlatilonU films is used in many different applications, such as the following:
    • Automotive: for the production of various interior trim parts e.g. headliners, door panels, seats, parcel shelves, sound insulation parts
    • Building & Construction: roof linings, pipe relining
    • Medical: colostomy bags, inflatable mattresses, antidecubitus mattresses, wound dressings, extra corporal breast prosthesis
    • Industrial: tank liners, air ducting, conveyor belts etc.
    • Sports and Leisure: sportswear, football outer skins and bladders, air cushions of athletic shoes etc.

    Information provided by Covestro

  • Vendors:
    Available Properties
    • Specific Gravity
    • Hardness, Shore A, ASTM D2240
    • Tensile Strength at Break, DIN EN ISO 527
    • Tensile Stress at Strain, DIN EN ISO 527
    • Elongation at Break, DIN EN ISO 527
    • Tear Strength, DIN ISO 34-1, B
    • Softening Point, TMA Onset
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    Covestro Deutschland AG, Bayer MaterialScience

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Visit Zeus Inc. for PEEK Tubing
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.