| KEBABLEND / TC FE 210601/8 PA is a special compound based on PA6, which is thermally and electrically conductive. Properties: thermally conductive Typical areas of application: Housing, Pumps and motors, Pump housing, Structural components, Connecting elements Industries: Automotive, Household appliances, Industry, Mechanical Engineering, Furniture industry Information provided by BARLOG plastics GmbH. |