MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Trinseo CALIBRE™ 891 20 Polycarbonate, General Purpose  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistance, high impact and are rated V-0 at 1.6 mm, 5V at 3.2 mm according to UL-94(1).

The CALIBRE 890 series resins are typically used in building and construction and in business equipment applications.

Available Melt Flow Rates: 10, 20

Associated products:
CALIBRE 891: including a mold release package
CALIBRE 893: including a mold release and UV stabilizer package.

These numerical flame spread ratings are small scale test values and are not intended to reflect hazards presented by these or any other materials under actual fire conditions.

Ignition resistant chemical additives increase resistance to burning from minor flame sources and permit properly manufactured end products to meet the requirements of certain flammability tests, but resins will burn rapidly under the right conditions of heat and oxygen feed.

Data provided by Dow Chemical.

Key Words: PC
Vendors:
Available Properties
  • Density, ASTM Data
  • Melt Density
  • Linear Mold Shrinkage
  • Melt Flow, ASTM Data
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate, ASTM Data
  • Tensile Strength, Yield, ISO Data
  • Elongation at Break, ASTM Data
  • Elongation at Yield, ISO Data
  • Tensile Modulus, ASTM Data
  • Izod Impact, Notched, ASTM Data
  • Charpy Impact, Notched, ISO Data, Low Temp
  • Charpy Impact, Notched, ISO Data
  • Instrumented Impact Total Energy
  • CTE, linear, Parallel to Flow, ASTM data
  • Specific Heat Capacity
  • Thermal Conductivity
  • Deflection Temperature at 1.8 MPa (264 psi), Unannealed; ASTM Data
  • Vicat Softening Point
  • Flammability, UL94, UL94
  • Oxygen Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.