MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
3M Scotch-Weld™ DP805 Acrylic Adhesives
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability and bond well to many metals, ceramics, wood and most plastics.

Information provided by 3M

Vendors:
Available Properties
  • Viscosity, Base
  • Viscosity, Accelerator
  • Hardness, Shore D
  • Tensile Strength at Break, ASTM D882
  • Elongation at Break, ASTM D882
  • Shear Strength, Overlap, CRS/CRS after 7 days of Immersion in MEK
  • Shear Strength, Overlap, CRS/CRS after 7 days of Immersion in Acetone
  • Shear Strength, Overlap, ABS
  • Shear Strength, Overlap, Aluminum -120 frit sandpaper
  • Shear Strength, Overlap, CRS/CRS tested after 120°C/2 wks
  • Shear Strength, Overlap, Aluminum -solvent cleaned only
  • Shear Strength, Overlap, Fiberglass Reinforced Plastic
  • Shear Strength, Overlap, Fir Wood
  • Shear Strength, Overlap, CRS/CRS after 7 days of Immersion in 10% HCl
  • Shear Strength, Overlap, Copper
  • Shear Strength, Overlap, Polycarbonate
  • Shear Strength, Overlap, Acrylic
  • Shear Strength, Overlap, Galvanized Steel
  • Shear Strength, Overlap, PVC
  • Shear Strength, Overlap, FR-4/FR-4 tested after tap water 1 wk/RT
  • Shear Strength, Overlap, CRS/CRS tested after 90°C/2 wks/90% RH
  • Shear Strength, Overlap, FR-4 Glass Epoxy
  • Shear Strength, Overlap, FR-4/FR-4 tested after RT aging
  • Shear Strength, Overlap, CRS/CRS tested after tap water 1 wk/RT
  • Shear Strength, Overlap, CRS/CRS after 7 days of Immersion in 1,1-Trichloroethane
  • Shear Strength, Overlap, FR-4/FR-4 tested after 90°C/2 wks/90% RH
  • Shear Strength, Overlap, CRS (oily) 49°C/100% RH/2 wks
  • Shear Strength, Overlap, CRS/CRS after 7 days of Immersion in Toluene
  • Shear Strength, Overlap, CRS/CRS after 7 days of Immersion in IPA
  • Shear Strength, Overlap, Cold Rolled Steel (oily)
  • Shear Strength, Overlap, FR-4/FR-4 tested after 120°C/2 wks
  • Shear Strength, Overlap, CRS/CRS after 7 days of Immersion in Gasoline
  • Shear Strength, Overlap, Cold Rolled Steel
  • Shear Strength, Overlap, Control
  • Shear Strength, Overlap, CRS/CRS tested after RT aging
  • Shear Strength, Overlap, CRS/CRS after 7 days of Immersion in Machine Oil
  • Shear Strength, Overlap, Etched Alum, 93°C/100% RH/2 wks
  • Shear Strength, Overlap, Aluminum-etched
  • Shear Strength, Overlap, Aluminum -etched/oily
  • Shear Strength, Overlap, Etched Alum (oily) 49°C/100% RH/4 wks
  • Shear Strength, Overlap, Etched Alum/Etched Alum
  • Shear Strength, Overlap, Etched Alum/Etched Alum
  • Shear Strength, Overlap, Etched Alum/Etched Alum
  • Peel Strength, 180° T-Peel, Black SBR/CRS
  • Peel Strength, 180° T-Peel, Nitrile/CRS
  • Peel Strength, 180° T-Peel, Neoprene/CRS
  • Peel Strength, 180° T-Peel, Red SBR/CRS
  • Peel Strength, 180° T-Peel, Etched Al/Etched Al
  • Peel Strength, 180° T-Peel, Etched Al/Etched Al
  • Peel Strength, 180° T-Peel, Etched Al/Etched Al
  • Peel Strength, 180° T-Peel, Etched Al/Etched Al
  • Peel Strength, 180° T-Peel, Etched Al/Etched Al
  • Peel Strength, 180° T-Peel, Etched Al/Etched Al
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear
  • Glass Transition Temp, Tg
  • Cure Time, Full cure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.