| Hifax EYC 335P C13055 is a 20% talc filled PP copolymer, with high flowability, low CLTE (Coefficient of Linear Thermal Expansion) and high impact resistance. Product is available as a customized color matched, pellet form. This grade is delivered in C13055 color version. Status: Commercial - Active Availability: Europe Application: Exterior Trim Market: Automotive Processing Method: Injection Molding Attribute: Good Color Stability; Good Dimensional Stability; Good Processability; Good UV Resistance; High Flow; High Impact Resistance Information provided by LyondellBasell. |