| TURBO-LOCK SERIES 10 is a removable, PURPLE, fast curing, low strength, anaerobic thread-locking compound for bonding and sealing small screw threads. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals. Easy disassembly. Applications: - Ideal for thread locking small screws from loosening under vibration.
- Ideal for fastening of ΒΌ" (6mm) and smaller diameters.
- Specifically suitable for applications such as adjustment of set screws and small diameter fasteners where easy disassembly is required.
- Meets Military specifications: MIL-S-46163
Part Numbers for this data: 10-001, 10-010, 10-050, 10-250, 10-1000 Information provided by Palm Laboratories Adhesives |
| CAS No: 923-26-2, 15625-89-5, 80-15-9 and 114-83-0 |