MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dow Dow™ DMDA-8904 NT 7 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow DMDA-8904 NT 7 HDPE is produced via UNIPOL™ Process Technology from Dow and is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. This resin has been designed to provide excellent processability for molders and to meet the rigorous performance characteristics of applications requiring stackabliity, environmental stress crack resistance and impact strength. This resin is also suitable for cast film extrusion processing.
  • Injection molding
  • For injection molded pails, industrial parts and other shipping containers
  • Excellent impact strength, stress crack resistance and processability
  • Very narrow molecular weight distribution.
Complies with: US FDA 21 CFR 177.1520©3.2a; EU, No 10/2011; Canadian HPFB No Objection. Consult the regulations for complete details.

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; EU No 10/2011; FDA 21 CFR 177.1520©3.2a; Canadian HPFB No Objection; UL 94

Form: Pellets

Processing Method: Cast Film; Injection Molding

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240, Molded and tested in accordance with ASTM D4976
  • Tensile Strength at Break, ASTM D638, Molded and tested in accordance with ASTM D4976
  • Tensile Strength, Yield, ASTM D638, Molded and tested in accordance with ASTM D4976
  • Elongation at Break, ASTM D638, Molded and tested in accordance with ASTM D4976
  • Elongation at Yield, ASTM D638, Molded and tested in accordance with ASTM D4976
  • Flexural Modulus, ASTM D790B, 2% Secant, Molded and tested in accordance with ASTM D4976
  • 2% Secant Modulus, ASTM D882, TD, Cast Film
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed, Molded and tested in accordance with ASTM D4976
  • Vicat Softening Point, ASTM D1525
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.