MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
MAS Epoxies LV RESIN FAST, MEDIUM & SLOW HARDENERS LV Resin Low Viscosity Laminating Epoxy System, Medium Hardener
Categories: Polymer; Thermoset; Epoxy

Material Notes: MAS Low Viscosity (LV) Resin with MAS Fast, Medium or Slow Hardeners is a non-blushing, low viscosity, low odor epoxy resin system. It can be used for laminating, filleting, and gluing. It has a simple 2 to 1 by volume mix ratio, easily wets out fiberglass fabric and requires no messy wash downs. MAS Fillers such as phenolic microballoons, colloidal silica or wood flour may be added to the epoxy resin to make compounds for bonding, fairing, filleting, or filling. LV Resin can be combined with FLAG Resin to create a custom viscosity resin. Fast, Medium and Slow Hardeners can be combined to create custom gel times. Easy to use 2:1 mix ratio by volume, Non-blushing system that requires no wash downs between laminations, Choose between three hardener speeds or mix them for custom gel times.

Information provided by MAS Epoxies.

Vendors:
Available Properties
  • Density, ASTM D1475, Hardener
  • Density, ASTM D792, Cured
  • Viscosity, ASTM D2196, Hardener
  • Viscosity, ASTM D2196, Initial Mixed
  • Viscosity, ASTM D2196, Resin
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Izod Impact, Notched, ASTM D256
  • Maximum Service Temperature, Air, ASTM D648, HDT load unknown, post cure
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg, ASTM D3418, Midpoint
  • Shrinkage, ASTM D792/2196 (volumetric)
  • Cure Time, Full cure
  • Tack-Free Time, Thin Film
  • Gel Time, ASTM D2471, 150g mass
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.