MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Covestro Baybond® PU 403 Polyester Urethane Polymer
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Baybond PU 403 is an anionic/non-ionic crosslinking polyester urethane polymer. It is used as the film-forming component in glass fiber sizes.

Properties / Applications: Baybond PU 403 was developed for the sizing of glass fibers used to reinforce thermoplastics, particularly polyamide. Glass fiber sizes based on Baybond PU 403 are characterized by their outstanding film-forming properties and very good adhesion. They have high colorfastness, even at elevated temperatures. The mechanical film properties of Baybond PU 403 are enhanced by post-crosslinking at temperatures from 170°C for a duration of 30 minutes. Baybond PU 403 is also very stable against shear forces. As with any product, use of Baybond PU 403 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors:
Available Properties
  • Density
  • Volatiles, 0.9-1.1g / 1h / 125°C, convection oven
  • Particle Size, Dv 0.5
  • Particle Size, Dv 0.9
  • Particle Size, Average
  • pH
  • Tensile Strength at Break
  • Elongation at Break
  • 100% Modulus
  • Glass Transition Temp, Tg
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.