MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik AQUA-CHEM® 896-9401 Aqueous Industrial Colorant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: AQUA-CHEM® 896 colorants are designed for use in a wide variety of water-based industrial coatings. The colorants are based upon a water-reducible acrylic resin. They can be used in water-reducible and emulsion coatings in both air-dry and baking systems. The colorants are low VOC and glycol-free. They have little or no effect on gloss, dry time, water resistance, hardness, corrosion, foaming, or other coating properties. AQUA-CHEM® 896 colorants are recommended for applications such as water-based general industrial, wood finishing, metal deco, architectural coatings, maintenance coatings for plastics, and rubber latex products.

896 Pigments: The pigments in these colorants were selected to provide a wide range of hues and good durability, lightfastness, and chemical resistance. However, the lightfastness, chemical and weathering properties of pigments depend a great deal on the coating in which they are used. The manufacturer recommends that, for positive verification of lightfastness and durability, the colorants be tested under accelerated and actual weathering conditions, to determine suitability for the desired use.

896 Tint Strength Control: 896 Colorants are controlled to a tinting strength tolerance of ±2% by volume. They are tested in a white base at a level of two fluid ounces per gallon. This close control allows for accurate reproduction of color. Rheological properties of the colorants are also controlled to allow for use in volumetric tinting machines. Volumetric formulas using 896 colorants are available for the ANSI Safety Colors and the Federal Standard 595b colors.

896 Intermix System Bases: The white tinting strength or TiO2 level for the white and deep bases used in the intermix system can be determined and adjusted as follows. Add the following levels of 896-0401 Red to the bases: White Base 124 oz. fill level, add 4 oz. of colorant Deep Base 120 oz. fill level, add 4 oz. of colorant These mixtures should be drawn down at 3 mil wet film thickness on sealed drawdown cards and compared to the base strength chips in the Industrial System fan deck.

Vendors:
Available Properties
  • Specific Gravity
  • Solids Content, vehicle
  • Solids Content, pigment
  • Volatile Organic Compounds (VOC) Content
  • Volatiles
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.