| Hifax TRC 835P JXW Black high melt flow, medium high flexural modulus, precolored, UV-stabilized, mineral filled, paintable thermoplastic elastomeric olefin (TEO) resin has a very good balance of properties. It is typically used for automotive exterior trim applications. Availability: North America Application: Automotive Parts; Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Information provided by LyondellBasell. |