MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik VESTAKEEP® Care M20 G PEEK, Medical Device Grade
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® Care is the ideal materials for the fabrication of medical devices with short time contact to human blood, tissue or bone for up to 30 days. VESTAKEEP® Care Grades have a good biocompatibility, processability and the option to pigment. VESTAKEEP® Care M20 G is a medium viscosity, unreinforced polyether ether ketone for injection molding. The semi-crystalline polymer features superior thermal and chemical resistance.
Dry properties listed below
Industrial Sector: Medical Devices
Processing: Injection molding
Delivery form: Pellets, Granules
Optics: Opaque
Resistance to: Heat (thermal stability), Hydrolysis / hot water, Oil / fuels
Conformity: Biocompatibility, Medical application
Additives: Unfilled
Applications: Encapsulation
Special Characteristics: Semi-crystalline
Regulatory: US Pharmacopeia Class VI conformity
Color: Natural color
Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistance

Information provided by Evonik.

Vendors:
Available Properties
  • Density, ISO 1183
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Melt Flow, ISO 1133
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527, Nominal
  • Elongation at Yield, ISO 527
  • Tensile Modulus, ISO 527
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Charpy Impact, Notched, ISO 179/1eA, Type of failure: C
  • Volume Resistivity, IEC 62631-3-1, ?V
  • Dielectric Constant, IEC 62631-2-1
  • Comparative Tracking Index, IEC 60112, test solution A, 50 drops value
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • Vicat Softening Point, ISO 306, 50 K/h
  • Vicat Softening Point, ISO 306, 50 K/h
  • Flammability, UL94, IEC 60695-11-10
  • Melt Temperature, ISO 294, Injection Molding
  • Mold Temperature, ISO 294, Injection Molding
  • Injection Velocity, ISO 294, Injection Molding
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.