MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Mitsubishi Xantar® 27 R Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances where quality is a key requirement. The Xantar® range includes:
  • clear and tinted grades for transparent applications
  • reinforced materials
  • Flame retardant and halogen free types
  • lubricated materials for added wear resistance

Mitsubishi Engineering Plastics acquired the Xantar® product line from DSM in 2010.

Vendors:
Available Properties
  • Density, ISO 1183
  • Water Absorption, Sim. to ISO 62
  • Viscosity Number, ISO 1628-4, Limiting Viscosity Number
  • Viscosity Number
  • Linear Mold Shrinkage, Flow, ISO 294-4
  • Melt Flow, ISO 1133, Calculated from Volume Flow Rate of 3 cm3/10min.
  • Hardness, Rockwell M, ISO 2039-2
  • Tensile Strength, Yield, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Elongation at Yield, ISO 527-1/-2
  • Tensile Modulus, ISO 527-1/-2
  • Flexural Strength, ISO 178
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched (ISO), ISO 180/4A
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • Comparative Tracking Index, UL 746A, PLC 2
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • Maximum Service Temperature, Air, IEC 60695-10-2, Ball Pressure Temperature
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Vicat Softening Point, ISO 306, 50°C/h 50N
  • UL RTI, Electrical, UL746B
  • UL RTI, Electrical, UL746B
  • UL RTI, Mechanical with Impact, UL746B
  • UL RTI, Mechanical with Impact, UL746B
  • UL RTI, Mechanical without Impact, UL746B
  • UL RTI, Mechanical without Impact, UL746B
  • Flammability, UL94, IEC 60695-11-10
  • Flammability, UL94, IEC 60695-11-10
  • Oxygen Index, ISO 4589-1/-2
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Ignition Temperature, IEC 60695-2-13
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Glow Wire Flammability Index, IEC 60695-2-12
  • Transmission, Visible, ASTM D1003, Light Transmittance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.